Optical constants of Biodisel
Wang et al. 2015: 60 °C; n,k 0.300–2.50 µm

Wavelength: µm
 (0.300–2.500)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 333

Notes

Biodiesel, 60 °C

References

C. C. Wang, X. C. Li, J. Y. Tan, L. H. Liu. Experimental measurement of optical constant of biodiesel by double optical pathlength transmission method. Laser Optoelectron. Prog. 52, 051206 (2015) (Numerical data kindly provided by Chengchao Wang)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Biodisel