Optical constants of C6H6 (Benzene)
Chang et al. 2024: n 0.4–2.0 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.180λ^2}{λ^2-0.138^2}$$Conditions
temperature: 295
Notes
21.5–22.0 °C
References
H.-J. Chang, N. Munera, C. Lopez-Zelaya, D. Banerjee, G. Beadie, E. W. Van Stryland, D. J. Hagan. Refractive index measurements of liquids from 0.5 to 2 µm using Rayleigh interferometry. Opt. Mater. Express 14, 1253–1267 (2024)
Data
Additional information
About Benzene
Benzene (C6H6) is a colorless and highly flammable liquid with a sweet smell. It's an aromatic hydrocarbon, notable for its cyclic, planar structure which consists of a hexagonal ring of carbon atoms, with alternating double and single bonds, and with a hydrogen atom bonded to each carbon. Benzene is used as a starting material in the manufacture of a vast array of chemicals, including styrene (for making polystyrene), phenol, and aniline. Its ring structure serves as a basis for many other chemical compounds and is fundamental in organic chemistry. However, exposure to benzene has been linked to a number of health concerns, particularly leukemia, leading to restrictions on its industrial and commercial use in many countries.
Other names and variations
- C6H6
- Cyclohexa-1,3,5-triene
- 1,3,5-Cyclohexatriene
- Benzol
- Phene
Links