Optical constants of ZrO2-Y2O3 (Yttria-stabilized zirconia, YSZ)
Wood and Nassau 1982: 12 mol % Y2O3; n 0.361–5.135 µm

Wavelength: µm
 (0.361–5.135)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{1.347091λ^2}{λ^2-0.062543^2}+\frac{2.117788λ^2}{λ^2-0.166739^2}+\frac{9.452943λ^2}{λ^2-24.320570^2}$$

Notes

Cubic zirconiza; 25 °C; Y2O3 content: 12.0 mol %

References

D. L Wood and K. Nassau. Refractive index of cubic zirconia stabilized with yttria. Appl. Opt. 21, 2978-2981 (1982)