Optical constants of ZrO2 (Zirconium dioxide, Zirconia)
Synowicki and Tiwald 2004: n,k 0.13–33 µm

Wavelength: µm
 (1.3010e-01–3.3000e+01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Data generated from oscillator model.

References

R.A. Synowicki and T. E. Tiwald. Optical properties of bulk c-ZrO2, c-MgO and a-As2S3 determined by variable angle spectroscopic ellipsometry. Thin Solid Films 455-456, 248-255 (2004)
Calculation scripts (Python): Synowicki 2004 - ZrO2.py, Synowicki 2004 - Aux funcs.py

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zirconium dioxide

Zirconium dioxide (ZrO2), often known as zirconia, is a white crystalline oxide of zirconium. Its most naturally occurring form, with a monoclinic crystalline structure, is the mineral baddeleyite. Zirconia is synthesized in various colors for use as a gemstone or in jewelry – cubic zirconia. The material's high melting point, chemical resistance, and low thermal conductivity make it a valuable component in various refractory applications. Additionally, its notable toughness and biocompatibility have made it a popular choice for dental ceramics and other biomedical applications, like hip implants. In optical applications, stabilized zirconia is used as a solid-state electrolyte in oxygen sensors and fuel cells due to its high oxygen ion conductivity.

Other names and variations

  • ZrO2
  • Zirconia
  • Zirconium(IV) oxide
  • Zirconium oxide

Links