Optical constants of ZrO2 (Zirconium dioxide, Zirconia)
Wood and Nassau 1982: Cubic zirconia stabilized with yttria; n 0.361–5.14 µm
Wavelength:
µm
(0.361–5.135)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.347091λ^2}{λ^2-0.062543^2}+\frac{2.117788λ^2}{λ^2-0.166739^2}+\frac{9.452943λ^2}{λ^2-24.320570^2}$$Notes
Cubic zirconiza; 25 °C; Y2O3 content: 12.0 mol %
References
D. L Wood and K. Nassau. Refractive index of cubic zirconia stabilized with yttria. Appl. Opt. 21, 2978-2981 (1982)
Data
Additional information
About Yttria-stabilized zirconia
Other names and variations
- YSZ
- ZrO2-Y2O3
- Zirconium dioxide - Yttrium oxide