Optical constants of ZnSe (Zinc selenide)
Querry 1987: n,k 0.500–21.7 µm
Complex refractive index (n+ik)
Derived optical constants
References
M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)
Data
Additional information
About Zinc selenide
Zinc selenide (ZnSe) is a binary compound semiconductor with a cubic zinc blende structure. This material is transparent in the visible and near-infrared regions of the electromagnetic spectrum, with a wide direct bandgap of approximately 2.7 eV. Due to its transparency and high refractive index, ZnSe has become a popular choice for high-power infrared laser systems, especially CO2 lasers, where ZnSe optics are used as output couplers and beam expanders. ZnSe can also be doped with various elements, most notably with chromium (Cr:ZnSe), to produce mid-infrared solid-state lasers. In addition, ZnSe is utilized in the fabrication of light-emitting diodes, photodetectors, and solar cells.
Other names and variations
- ZnSe
Links