Optical constants of ZnS (Zinc sulfide)
Querry 1987: n,k 0.220–167 µm

Wavelength: µm
 (0.2200–166.6667)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

References

M. R. Querry. Optical constants of minerals and other materials from the millimeter to the ultraviolet, Contractor Report CRDEC-CR-88009 (1987)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc sulfide

Zinc sulfide (ZnS) is a semiconducting material that exhibits either a sphalerite (cubic) or wurtzite (hexagonal) crystal structure. It has a direct bandgap of around 3.68 eV for the cubic form and 3.91 eV for the hexagonal form. Due to its luminescent properties, ZnS has been extensively used in applications like electroluminescent panels, X-ray screens, and phosphorescent materials. Doped ZnS, especially with copper or silver, can produce phosphorescent materials widely used in various displays. ZnS is also employed as a host matrix in many quantum dot applications. Additionally, its infrared transmission capability makes it valuable for infrared optics, and it's frequently used in infrared windows and lenses.

Minerals: Sphalerite (mineral of cubic ZnS), Wurtzite (mineral of hexagonal ZnS)