Optical constants of ZnS (Zinc sulfide)
Ozaki and Adachi 1993: Cubic ZnS; n,k 0.221–1.03 µm

Wavelength: µm
 (2.2140e-01–1.0332e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Fit of author's experimental data to a simplified model of the interband transitions (MDF). Room Temperature.

References

S. Ozaki and S. Adachi. Optical constants of cubic ZnS. Jpn. J. Appl. Phys. 32, 5008-5013 (1993)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc sulfide

Zinc sulfide (ZnS) is a semiconducting material that exhibits either a sphalerite (cubic) or wurtzite (hexagonal) crystal structure. It has a direct bandgap of around 3.68 eV for the cubic form and 3.91 eV for the hexagonal form. Due to its luminescent properties, ZnS has been extensively used in applications like electroluminescent panels, X-ray screens, and phosphorescent materials. Doped ZnS, especially with copper or silver, can produce phosphorescent materials widely used in various displays. ZnS is also employed as a host matrix in many quantum dot applications. Additionally, its infrared transmission capability makes it valuable for infrared optics, and it's frequently used in infrared windows and lenses.

Minerals: Sphalerite (mineral of cubic ZnS), Wurtzite (mineral of hexagonal ZnS)

Other names and variations

  • ZnS
  • Zinc sulphide
  • Zinc blende
  • Sphalerite
  • Wurtzite