Optical constants of ZnO-CdO (Zinc cadmium oxide, ZnCdO)
Aguilar et al. 2019: n,k 0.3–3.2 µm; 40% ZnO

Wavelength: µm
 (0.300–3.200)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Zn0.4Cd0.6O (40% ZnO, 60% CdO) thin film.

References

O. Aguilar, S. de Castro, M. P. F. Godoy, M. R. S. Dias. Optoelectronic characterization of Zn1-xCdxO thin films as an alternative to photonic crystals in organic solar cells. Opt. Mater. Express 9, 3638-3648 (2019) (Numerical data kindly provided by Mariama Rebello de Sousa Dias)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc-cadmium oxide

Other names and variations

  • ZnCdO
  • ZnO-CdO

Links