RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ZnO (Zinc monoxide)
Bodurov et al. 2016: Nanoparticles; n 0.405–0.635 µm

Wavelength: µm
 (0.405–0.635)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.7820λ^2}{λ^2-0.0842380^2}$$

Conditions

temperature: 297

Notes

<50 nm diameter nanoparticles dispersed in water. Concentration 50 wt.%. 24 °C. Refractive index of nanoparticles calculated using Bruggeman's effective medium approximation.

References

I. Bodurov, I. Vlaeva, A. Viraneva, T. Yovcheva, S. Sainov. Modified design of a laser refractometer, Nanoscience & Nanotechnology 16, 31-33 (2016)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc monoxide

Zinc oxide (ZnO) is a direct bandgap semiconductor with a wide bandgap of approximately 3.37 eV. This unique property makes it a material of significant interest for various optoelectronic applications, including solar cells, sensors, and LEDs. ZnO also exhibits piezoelectric properties, which are exploited in the design of sensors and actuators. It naturally forms in a hexagonal wurtzite crystal structure, displaying strong luminescence even at room temperature. Additionally, ZnO is a transparent conductive oxide, meaning it conducts electricity while remaining transparent to visible light, making it useful in transparent electronics and touchscreens. Due to its antibacterial and UV-blocking properties, ZnO is also commonly used as an ingredient in cosmetics and sunscreens.

Other names and variations

  • ZnO
  • Zinc(II) oxide
  • Zinc oxide
  • Zinc white
  • Calamine

Links