Optical constants of ZnGeP2 (Zinc germanium phosphide, ZGP)
Zelmon et al. 2001: n(o) 2–9 µm

Wavelength: µm
 (2–9)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=7.0409+\frac{1.68625λ^2}{λ^2-0.40824}+\frac{1.2880λ^2}{λ^2-611.05}$$

Conditions

temperature: 294
optical_component: o

Notes

Ordinary optical constants (o); 21-22 °C.

References

D. E. Zelmon, E. A. Hanning, P. G. Schunemann. Refractive-index measurements and Sellmeier coefficients for zinc germanium phosphide from 2 to 9 µm with implications for phase matching in optical frequency-conversion devices. J. Opt. Soc. Am. B 18, 1307-1310 (2001)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc germanium phosphide

Zinc germanium phosphide (ZnGeP2, ZGP), is a non-linear optical material that has been widely used for frequency conversion in the mid-infrared range. It possesses a broad transparency range, high damage threshold, and phase-matching capabilities, making it a favored choice for a variety of laser applications. Owing to its ability to efficiently generate coherent radiation in the 2 to 12 µm spectral range, ZGP is especially relevant for molecular spectroscopy, environmental monitoring, and medical surgery. As a non-centrosymmetric crystal, ZGP can be employed for second harmonic generation, parametric oscillation, and other non-linear processes when exposed to suitable pump sources.