RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ZnGeP2 (Zinc germanium phosphide, ZGP)
Ghosh 1998: n(o) 0.7–12 µm; 100 K

Wavelength: µm
 (0.7–12)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=3.49338530+\frac{5.10900476λ^2}{λ^2-0.12778958}+\frac{2.16855561λ^2}{λ^2-900}$$

Conditions

temperature: 100
optical_component: o

Notes

Critical analysis of experimental data from multiple sources.

References

G. Ghosh. Sellmeier coefficients for the birefringence and refractive indices of ZnGeP2 nonlinear crystal at different temperatures. Appl. Opt., 37, 1205-1212 (1998)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc germanium phosphide

Zinc germanium phosphide (ZnGeP2, ZGP), is a non-linear optical material that has been widely used for frequency conversion in the mid-infrared range. It possesses a broad transparency range, high damage threshold, and phase-matching capabilities, making it a favored choice for a variety of laser applications. Owing to its ability to efficiently generate coherent radiation in the 2 to 12 µm spectral range, ZGP is especially relevant for molecular spectroscopy, environmental monitoring, and medical surgery. As a non-centrosymmetric crystal, ZGP can be employed for second harmonic generation, parametric oscillation, and other non-linear processes when exposed to suitable pump sources.

Other names and variations

  • ZnGeP2
  • ZGP
  • Zinc germanium diphosphide

Links