RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ZnGeP2 (Zinc germanium phosphide, ZGP)
Das et al. 2003: n(e) 1.32–11 µm

Wavelength: µm
 (1.32–11)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=2.65014+\frac{6.310153λ^2}{λ^2-0.125099}+\frac{1.731381λ^2}{λ^2-900}$$

Conditions

optical_component: e

Notes

Extraordinary optical constants (e)

References

S. Das, G. C. Bhar, S. Gangopadhyay, C. Ghosh. Linear and nonlinear optical properties of ZnGeP2 crystal for infrared laser device applications: Revisited. Appl. Opt. 42, 4335-4340 (2003)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Zinc germanium phosphide

Zinc germanium phosphide (ZnGeP2, ZGP), is a non-linear optical material that has been widely used for frequency conversion in the mid-infrared range. It possesses a broad transparency range, high damage threshold, and phase-matching capabilities, making it a favored choice for a variety of laser applications. Owing to its ability to efficiently generate coherent radiation in the 2 to 12 µm spectral range, ZGP is especially relevant for molecular spectroscopy, environmental monitoring, and medical surgery. As a non-centrosymmetric crystal, ZGP can be employed for second harmonic generation, parametric oscillation, and other non-linear processes when exposed to suitable pump sources.

Other names and variations

  • ZnGeP2
  • ZGP
  • Zinc germanium diphosphide

Links