Optical constants of ZBLAN fluoride glass
Gan 1995: n 0.365–3.50 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{1.22514λ^2}{λ^2-0.08969^2}+\frac{1.52898λ^2}{λ^2-21.3825^2}$$Notes
Room temperature.
References
F. Gan. Optical properties of fluoride glasses: a review. J. Non-Cryst. Solids 184, 9–20 (1995)
Data
Additional information
About ZBLAN fluoride glass
ZBLAN is a type of heavy-metal fluoride glass composed primarily of zirconium, barium, lanthanum, aluminum, and sodium fluorides. It is distinguished by its exceptional transmission capabilities in the mid-infrared range, often far superior to that of silica-based glasses. ZBLAN glass is renowned for its low levels of optical scattering, low refractive index variations, and low optical losses, making it an ideal material for fiber-optic applications, especially for those operating in the infrared spectrum. It also boasts a broad transmission window, from the ultraviolet through to the mid-infrared, and is often used in applications like spectroscopy, laser transmission, and sensing where these properties offer distinct advantages. However, ZBLAN can be challenging to manufacture and work with due to its sensitivity to impurities and crystallization. Despite these challenges and its relatively high cost, the unique optical properties of ZBLAN make it indispensable for specialized applications where conventional optical materials fall short.
Typical composition: 53% ZrF4, 20% BaF2, 20% NaF, 4% LaF3, 3% AlF3
Links