Optical constants of Yb2O3 (Ytterbium sesquioxide)
Medenbach et al. 2001: n 0.435–0.644 µm

Wavelength: µm
 (0.435–0.644)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.647λ^2}{λ^2-0.01800}$$

References

O. Medenbach, D. Dettmar, R. D. Shannon, R. X. Fischer, W. M. Yen. Refractive index and optical dispersion of rare earth oxides using a small-prism technique. J. Opt. A: Pure Appl. Opt. 3, 174-177, 2001

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Ytterbium sesquioxide

Ytterbium sesquioxide (Yb2O3) is a chemical compound formed from ytterbium and oxygen. This white, crystalline oxide is one of the primary compounds of ytterbium and serves as a common precursor in the preparation of other ytterbium salts. Its high melting point and stable nature make it a suitable material for certain specialized applications. In the realm of optics and photonics, Yb2O3-doped materials are of interest for their lasing properties, especially when doped into laser host materials. The compound is also researched in the context of high-temperature superconductors and other advanced materials. Being an oxide of a rare-earth element, Yb2O3 shares many characteristics typical of the lanthanide series, including its ability to form complex coordination compounds.