RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of YVO4 (Yttrium orthovanadate)
Shi et al. 2001: n(e) 0.48–1.34 µm; 140 °C

Wavelength: µm
 (0.48–1.34)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=4.613554+\frac{0.017202}{λ^2-0.055974}-0.014652λ^{2}$$

Conditions

temperature: 413
optical_component: e

Notes

Extraordinary optical constants (e), 140 °C.

References

H. S. Shi, G. Zhang and H. Y. Shen. Measurement of principal refractive indices and the thermal refractive index coefficients of yttrium vanadate. J. Synthetic Cryst. 30, 85-88 (2001)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Yttrium orthovanadate

Yttrium orthovanadate (YVO4) is a crystalline material known for its outstanding optical properties. It serves as a prominent choice for optical applications, especially as a laser host crystal. When doped with specific rare-earth ions like neodymium (Nd:YVO4), it becomes a popular solid-state laser medium due to its high gain, low lasing threshold, and high efficiency. YVO4 also exhibits excellent birefringence, which makes it suitable for frequency doubling and other nonlinear optical processes. The material boasts a broad transparency range, from the visible to the near-infrared spectrum. Its high index of refraction enables tight focusing of light, beneficial in certain optical systems. In its pure form, YVO4 is transparent and colorless.

Other names and variations

  • YVO4
  • Yttrium vanadate

Links