Optical constants of YVO4 (Yttrium orthovanadate)
Birnbaum and DeShazer 1976: n(e) 0.488–3.39 µm

Wavelength: µm
 (0.488–3.39)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{3.5930λ^2}{λ^2-0.032103}$$

Conditions

optical_component: e

Notes

Extraordinary optical constants (e)

References

  1. M. Birnbaum, L. G. DeShazer. Low threshold CW Nd laser oscillator at 1060 nm study. NASA Report, Contract Number NAS 5-22387 (1976)
  2. T. S. Lomheim. L. G. DeShazer. Optical-absorption intensities of trivalent neodymium in the uniaxial crystal yttrium orthovanadate. J. Appl. Phys. 49, 5517-5522 (1978)
  • Ref. 2 provides a dispersion formula based on data from Ref. 1

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Yttrium orthovanadate

Yttrium orthovanadate (YVO4) is a crystalline material known for its outstanding optical properties. It serves as a prominent choice for optical applications, especially as a laser host crystal. When doped with specific rare-earth ions like neodymium (Nd:YVO4), it becomes a popular solid-state laser medium due to its high gain, low lasing threshold, and high efficiency. YVO4 also exhibits excellent birefringence, which makes it suitable for frequency doubling and other nonlinear optical processes. The material boasts a broad transparency range, from the visible to the near-infrared spectrum. Its high index of refraction enables tight focusing of light, beneficial in certain optical systems. In its pure form, YVO4 is transparent and colorless.