Optical constants of Y3Al5O12 (Yttrium aluminium garnet, YAG)
Zelmon et al. 1998: n 0.4–5.0 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{2.28200λ^2}{λ^2-0.01185}+\frac{3.27644λ^2}{λ^2-282.734}$$References
D. E. Zelmon, D. L. Small and R. Page. Refractive-index measurements of undoped yttrium aluminum garnet from 0.4 to 5.0 μm. Appl. Opt. 37, 4933-4935 (1998)
Data
Additional information
About Yttrium aluminium garnet
Yttrium aluminium garnet (Y3Al5O12, YAG) is a synthetic crystalline material frequently employed in a variety of applications. It possesses a unique combination of high thermal stability, mechanical robustness, and optical clarity, making it particularly desirable for high-performance environments. In the realm of optics and photonics, YAG is often used as the host crystal in solid-state lasers, most notably the Nd:YAG laser where the YAG crystal is doped with neodymium. These lasers are employed in a range of settings, from medical procedures to material processing. Additionally, undoped YAG is a common substrate for various thin-film applications, given its compatibility with high-temperature deposition processes. In the lighting sector, YAG, when doped with cerium, is used as a phosphor in white LED technology.
Other names and variations
- Y3Al5O12
- YAG
- Yttrium aluminate
- Yttrium aluminium oxide
Links