Optical constants of Y3Al5O12 (Yttrium aluminium garnet, YAG)
Bond 1965: n 0.4–4.0 µm
Complex refractive index (n+ik)
Derived optical constants
Notes
Room temperature.
References
W. L. Bond. Measurement of the refractive indices of several crystals. J. Appl. Phys. 36, 1674-1677 (1965)
Data
Additional information
About Yttrium aluminium garnet
Yttrium aluminium garnet (Y3Al5O12, YAG) is a synthetic crystalline material frequently employed in a variety of applications. It possesses a unique combination of high thermal stability, mechanical robustness, and optical clarity, making it particularly desirable for high-performance environments. In the realm of optics and photonics, YAG is often used as the host crystal in solid-state lasers, most notably the Nd:YAG laser where the YAG crystal is doped with neodymium. These lasers are employed in a range of settings, from medical procedures to material processing. Additionally, undoped YAG is a common substrate for various thin-film applications, given its compatibility with high-temperature deposition processes. In the lighting sector, YAG, when doped with cerium, is used as a phosphor in white LED technology.
Other names and variations
- Y3Al5O12
- YAG
- Yttrium aluminate
- Yttrium aluminium oxide