Optical constants of Xe (Xenon)
Bideau-Mehu et al. 1981: n 0.140–0.623 µm

Wavelength: µm
 (0.1404–0.6234)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=\frac{0.00322869}{46.301-λ^{-2}}+\frac{0.00355393}{59.578-λ^{-2}}+\frac{0.0606764}{112.74-λ^{-2}}$$

Conditions

temperature: 273.15
pressure: 101325

Notes

Standard conditions: 0 °C, 760 torr (101.325 kPa).

References

  1. A. Bideau-Mehu, Y. Guern, R. Abjean, A. Johannin-Gilles. Measurement of refractive indices of neon, argon, krypton and xenon in the 253.7-140.4 nm wavelength range. Dispersion relations and estimated oscillator strengths of the resonance lines. J. Quant. Spectrosc. Rad. Transfer 25, 395-402 (1981)

  2. J. Koch. Kungl. Fysiografiska Sällskapets i Lund Förhandlingar (Proceedings of the Royal Physiographic Society at Lund) 19, 173 (1949)
  • Sellmeier formula is derived by the authors of ref. 1 using their own data in the 0.1404-0.2537 μm range combined with data from ref. 2 at longer wavelengths.
    ** A misprint is corrected in the Sellmeier formula: "50.578" is replaced by "59.578" in the denominator of the second term.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Xenon

Xenon (Xe) is a noble gas that exists as a colorless, dense, odorless gas under standard conditions. It's one of the rare gases found in the Earth's atmosphere, representing only a tiny fraction of the air we breathe. Due to its heavy atomic weight and low reactivity, xenon is often used in specialized lighting, including powerful flash lamps, high-intensity arc-lamps, and as the propellant in ion engines for deep space missions. In medicine, xenon has been explored as an anesthetic and in imaging. Its isotopes also find use in various applications, such as the detection of neutrinos in particle physics experiments. Xenon can form compounds, albeit rarely, with highly electronegative elements like fluorine.

Other names and variations

  • Xe

Links