RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of WSe2 (Tungsten diselenide)
Hsu et al. 2019: 3-layer (3L) film; n,k 0.40–0.85 µm

Wavelength: µm
 (0.39697–0.85024)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 3L

Notes

3-layer (3L)

References

C. Hsu, R. Frisenda, R. Schmidt, A. Arora, S. M. de Vasconcellos, R. Bratschitsch, H. S. J. van der Zant, A. Castellanos-Gomez. Thickness-dependent refractive index of 1L, 2L, and 3L MoS2, MoSe2, WS2, and WSe2. Adv. Optical Mater. 7, 1900239 (2019) (Numerical data kindly provided by Andres Castellanos-Gomez)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tungsten diselenide

Tungsten diselenide (WSe2) is a member of the transition metal dichalcogenide (TMD) family, known for its distinctive layered structure. The individual layers are bound by weak van der Waals interactions, allowing for exfoliation into atomically thin sheets. In its monolayer form, WSe2 possesses a direct bandgap, distinguishing it from its bulk indirect bandgap property. This unique characteristic renders WSe2 as a prime candidate for optoelectronic applications, including photodetectors, light-emitting diodes (LEDs), and even photovoltaic devices. It has also been explored in the fabrication of field-effect transistors and quantum devices. The intriguing electronic and optical attributes of WSe2, especially when interfaced with other 2D materials, have garnered significant attention in advanced materials research.

Other names and variations

  • WSe2

Links