Optical constants of WS2 (Tungsten disulfide)
Hsu et al. 2019: 2-layer (2L) film; n,k 0.40–0.85 µm
Complex refractive index (n+ik)
Derived optical constants
Conditions
film_thickness: 2L
Notes
2-layer (2L)
References
C. Hsu, R. Frisenda, R. Schmidt, A. Arora, S. M. de Vasconcellos, R. Bratschitsch, H. S. J. van der Zant, A. Castellanos-Gomez. Thickness-dependent refractive index of 1L, 2L, and 3L MoS2, MoSe2, WS2, and WSe2. Adv. Optical Mater. 7, 1900239 (2019) (Numerical data kindly provided by Andres Castellanos-Gomez)
Data
Additional information
About Tungsten disulfide
Tungsten disulfide (WS2) is a layered transition metal dichalcogenide that possesses distinct properties based on its structural morphology. In its three-dimensional bulk form, WS2 has indirect bandgap semiconducting properties, which contrasts its behavior when isolated to a monolayer or few-layer forms. When exfoliated to these thin layers, WS2 undergoes a transition to a direct bandgap semiconductor, making it intriguing for potential applications in electronics, optoelectronics, and photonics. This material's unique hexagonal structure gives it excellent lubrication capabilities, often preferred in environments with high pressures and temperatures. Furthermore, research continues into its promise in nanoelectronic devices, spintronic applications, and as a component in heterostructures with other two-dimensional materials.
Other names and variations
- WS2
Links