Optical constants of WO3 (Tungsten trioxide)
Kulikova et al. 2020: n,k 0.3–1.0 µm

Wavelength: µm
 (0.300–1.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 8.1E-8
substrate: SiO2

Notes

81 nm-thick WO3 film deposited directly on SiO2 substrate

References

D.P. Kulikova, A.A. Dobronosova, V.V. Kornienko, I.A. Nechepurenko, A.S. Baburin, E.V. Sergeev, E.S. Lotkov, I.A. Rodionov, A.V. Baryshev, A.V. Dorofeenko. Optical properties of tungsten trioxide, palladium, and platinum thin films for functional nanostructures engineering. Opt. Express 28, 32049-32060 (2020) (Numerical data kindly provided by Alexander Dorofeenko)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tungsten trioxide

Tungsten trioxide (WO3) is a compound of tungsten and oxygen that presents as a yellow, inorganic solid in its pure form. It has notable photochromic properties, meaning it can change color upon exposure to light. Due to this unique characteristic, WO3 has been explored for use in smart windows that can modulate the amount of light they let through based on external conditions. Additionally, it's an essential material in the field of electrochromism, with potential applications in electrochromic devices like smart windows and displays. Tungsten trioxide is also used as a precursor for the synthesis of other tungsten compounds and is employed as a raw material in the production of tungsten metal. Furthermore, it plays a role in catalysis, particularly in processes that involve the oxidation of volatile organic compounds.

Other names and variations

  • WO3
  • Tungstic anhydride
  • Tungsten(VI) oxide
  • Tungsten oxide
  • Tungstic oxide
  • Trioxotungsten

Links