RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of W (Tungsten)
Werner et al. 2009: DFT calculations; n,k 0.0176–2.48 µm

Wavelength: µm
 (0.017586–2.479684)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Theoretical density function theory (DFT) calculations.

References

W. S. M. Werner, K. Glantschnig, C. Ambrosch-Draxl. Optical constants and inelastic electron-scattering data for 17 elemental metals. J. Phys Chem Ref. Data 38, 1013-1092 (2009)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tungsten

Tungsten, commonly known by its chemical symbol W (derived from its alternative name, wolfram), is a hard, dense metal with a bright silver-gray luster. Known for its high melting point, which is the highest of all the elements at 3,422°C (6,192°F), tungsten is often used in applications that require materials that can withstand extreme temperatures. Historically, it's been a crucial component in the filaments of incandescent light bulbs. Moreover, tungsten and its alloys are utilized in many high-temperature structural materials, particularly in aerospace and electronic industries due to their remarkable strength at elevated temperatures. Tungsten is also used in the production of wear-resistant electrical contacts and as the primary component in certain types of heavy metal alloys. In the realm of optics and photonics, tungsten is often used as a target for X-ray generation.

Other names and variations

  • W

Links