RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of W (Tungsten)
Rakić et al. 1998: Brendel-Bormann model; n,k 0.248–12.4 µm

Wavelength: µm
 (2.4797e-01–1.2398e+01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Fit of experimental data from several sources to Brendel-Bormann (BB) model

References

A. D. Rakić, A. B. Djurišic, J. M. Elazar, and M. L. Majewski. Optical properties of metallic films for vertical-cavity optoelectronic devices. Appl. Opt. 37, 5271-5283 (1998)
[
Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tungsten

Tungsten, commonly known by its chemical symbol W (derived from its alternative name, wolfram), is a hard, dense metal with a bright silver-gray luster. Known for its high melting point, which is the highest of all the elements at 3,422°C (6,192°F), tungsten is often used in applications that require materials that can withstand extreme temperatures. Historically, it's been a crucial component in the filaments of incandescent light bulbs. Moreover, tungsten and its alloys are utilized in many high-temperature structural materials, particularly in aerospace and electronic industries due to their remarkable strength at elevated temperatures. Tungsten is also used in the production of wear-resistant electrical contacts and as the primary component in certain types of heavy metal alloys. In the realm of optics and photonics, tungsten is often used as a target for X-ray generation.

Other names and variations

  • W

Links