RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of VITRON - Infrared glass (IG)
IG 3

Wavelength: µm
 (1–14.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=3.885429+\frac{2.934475λ^2}{λ^2-0.508386^2}+\frac{0.573772λ^2}{λ^2-32.406166^2}$$

Notes

Room temperature. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.

References

  1. VITRON datasheet IG-3 June 2014
  2. Dr. Rolf Henkel (VITRON Spezialwerkstoffe GmbH) - private communications

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information