Optical constants of VITRON - Infrared glass (IG)
IG 2
Wavelength:
µm
(1–14.0)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2-1=2.341388+\frac{2.962098λ^2}{λ^2-0.360017^2}+\frac{0.831035λ^2}{λ^2-35.023342^2}$$Notes
Room temperature. Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers.
References
- VITRON datasheet IG-2 June 2014
- Dr. Rolf Henkel (VITRON Spezialwerkstoffe GmbH) - private communications