Optical constants of VC (Vanadium carbide)
Pflüger et al. 1984: n,k 0.0311–2.48 µm
Wavelength:
µm
(0.03107–2.4797)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
VC0.88. Room temperature.
References
- J. Pflüger, J. Fink.
Determination of optical constants by high-energy, electron-energy-loss spectroscopy (EELS), in Handbook of optical constants of solids II, Edward D. Palik, ed. Academic Press, 1991. pp. 293-310
- J. Pflüger, J. Fink, W. Weber, K. P. Bohnen, G. Crecelius. Dielectric properties of TiCx, TiNx, VCx, and VNx from 1.5 to 40 eV determined by electron-energy-loss spectroscopy. Phys. Rev. B 30, 1155-1163 (1984)
Data
Additional information
About Vanadium carbide
Vanadium carbide (VC) is a hard, refractory ceramic compound composed of vanadium and carbon. It is an extremely hard material, with a hardness value that can rival that of diamond. This makes it a valuable additive in tool steels, where it provides increased wear resistance. Furthermore, VC can be used as a grain growth inhibitor, preventing grains from growing too large during the heat-treating process, which can be beneficial in achieving desired material properties in metallurgical applications. Additionally, vanadium carbide can also be found in coatings, often applied through processes like physical vapor deposition (PVD) to provide wear resistance in tools and parts.
Other names and variations
- VC
- Vanadium(IV) carbide
- Vanadium carbon
Links