Optical constants of Tm (Thulium)
Vidal-Dasilva et al. 2009: n,k 0.000775–0.480 µm
Complex refractive index (n+ik)
Derived optical constants
Comments
Density: 9.33 g/cm3. Film deposited at room temperature.
References
M. Vidal-Dasilva, M. Fernández-Perea, J. A. Aznárez, J. I. Larruquert, J. A. Méndez, L. Poletto, A. M. Malvezzi, A. Giglia, S. Nannarone. Transmittance and optical constants of Tm films in the 2.75–1600 eV spectral range. J. Appl. Phys. 105, 103110 (2009) (Numerical data kindly provided by Juan Larruquert)
Data
Additional information
About Thulium
Thulium (Tm) is a rare-earth metal, belonging to the lanthanide series of the periodic table. It is silvery-white and soft, displaying properties common to most of the rare-earth elements. Thulium can be isolated from other rare earths through ion-exchange reactions. While thulium is not as abundant or widely used as other rare earths, it has several niche applications. One of its artificially-produced isotopes, Tm-170, is employed as a radiation source in portable X-ray devices. Additionally, thulium lasers, specifically Tm:YAG lasers, have applications in medical procedures, industrial drilling, and research.
Other names and variations
- Tm
Links