RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of TlBr (Thallium bromide)
Palik 1985: n 0.57–39.4 µm

Wavelength: µm
 (0.57–39.4)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{3.7442390λ^2}{λ^2-0.2079603^2}+\frac{0.9189162λ^2}{λ^2-0.3765643^2}+\frac{12.5444602λ^2}{λ^2-165.6525518^2}$$

Notes

25 °C

References

Handbook of Optical Constants of Solids, Edward D. Palik, ed. Academic Press, Boston, 1985

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Thallium bromide

Thallium bromide (TlBr) is a crystalline compound with interesting properties that make it suitable for radiation detection applications. It possesses a wide bandgap and high atomic numbers for both thallium and bromine, characteristics that enhance its performance as a gamma-ray detector. Additionally, TlBr detectors exhibit high energy resolution and are suitable for high-temperature operations. Due to its potential in radiation detection, TlBr has attracted attention in the field of nuclear medicine and security. However, the material's long-term stability and potential toxicity from thallium content require careful consideration during usage and handling.

Other names and variations

  • TlBr
  • Thallium(I) bromide

Links