Optical constants of TiO2 (Titanium dioxide)
Devore 1951: n(o) 0.43–1.53 µm

Wavelength: µm
 (0.43–1.53)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=5.913+\frac{0.2441}{λ^2-0.0803}$$

Conditions

optical_component: o

Notes

Ordinary optical constants (o); Room temperature.

References

J. R. Devore. Refractive indices of rutile and sphalerite. J. Opt. Soc. Am. 41, 416-419 (1951)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Titanium dioxide

Titanium dioxide (TiO2) is a naturally occurring oxide of titanium. It possesses a high refractive index, making it an important material in optical coatings and components, especially as a white pigment in paints, cosmetics, and sunscreens due to its UV absorbing properties. The two main crystal forms used in industry are the rutile and anatase forms. Additionally, its photovoltaic and photocatalytic properties have led to research and applications in solar cells and air purification, respectively. TiO2 also has a robust chemical stability under various conditions, which makes it a preferred material for use in harsh environments.

Minerals: Rutile, Anatase, Brookite.