Optical constants of TiN (Titanium nitride)
Pflüger et al. 1984: n,k 0.031–2.48 µm
Complex refractive index (n+ik)
Derived optical constants
Conditions
substrate: Mo
Notes
TiN1.0 film on Mo substratre. Room temperature.
References
- J. Pflüger, J. Fink.
Determination of optical constants by high-energy, electron-energy-loss spectroscopy (EELS),
in Handbook of optical constants of solids II, Edward D. Palik, ed. Academic Press, 1991. pp. 293-310
- J. Pflüger, J. Fink, W. Weber, K. P. Bohnen, G. Crecelius. Dielectric properties of TiCx, TiNx, VCx, and VNx from 1.5 to 40 eV determined by electron-energy-loss spectroscopy. Phys. Rev. B 30, 1155-1163 (1984)
Data
Additional information
About Titanium nitride
Titanium nitride (TiN) is a hard ceramic material characterized by its golden appearance. Due to its high hardness and resistance to wear, TiN is commonly used as a coating on tools, such as drill bits and end mills, to extend their life and improve their performance. The coating also exhibits a low coefficient of friction, which reduces galling and seizing. Moreover, its corrosion resistance makes it suitable for biomedical applications, such as coatings on surgical instruments and orthopedic implants. In electronics, TiN serves as a barrier layer between metals in integrated circuits. It's typically deposited using physical vapor deposition (PVD) or chemical vapor deposition (CVD) techniques. Additionally, its metallic luster and gold hue make it a popular decorative coating for architectural and consumer products.