RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Therminol VP-1
Otanicar et al. 2009: k 0.2–1.5 µm

Wavelength: µm
 (0.20–1.50)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

25 °C

References

T. P. Otanicar, P. E. Phelan J. S. Golden. Optical properties of liquids for direct absorption solar thermal energy systems. Solar Energy 83, 969-977 (2009)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Heat transfer fluids