RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of TaS2 (Tantalum disulfide)
Munkhbat et al. 2022: multilayer flakes; n,k(o) 0.30–1.69 µm

Wavelength: µm
 (3.000000e-01–1.690000e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: o

Notes

Multilayer flakes. In-plane (ordinary ray, o). Room temperature.

References

B. Munkhbat, P. Wrobel, T. J. Antosiewicz, T. O. Shegai. Optical constants of several multilayer transition metal dichalcogenides spectroscopic ellipsometry in the 300–1700 nm range: High index, anisotropy, and hyperbolicity. ACS Photonics 9, 2398–2407 (2022) (Numerical data kindly provided by Tomasz Antosiewicz)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Tantalum disulfide

Tantalum disulfide (TaS2) is a layered transition metal dichalcogenide with intriguing electrical and optical properties. It's known for its charge density wave (CDW) transitions, which can lead to various electronic states, such as metallic, insulating, and superconducting phases. This material is also of considerable interest in the research community for its potential in miniaturized electronic devices and as a platform for studying correlated electron systems. The thin layers of TaS2 can be exfoliated, making it a candidate for use in nanoscale electronic and optoelectronic applications. The compound's unique electronic properties also make it a subject of interest in the exploration of novel quantum phenomena.

Other names and variations

  • TaS2
  • Tantalum(IV) sulfide

Links