Optical constants of TL-216
Li et al. 2005: n(e) 0.450–0.656 µm
Wavelength:
µm
(0.45–0.656)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.6772+0.0155λ^{-2}+0.0011λ^{-4}$$Conditions
temperature: 298 optical_component: e
Notes
25 °C. Extraordinary optical constants (e).
References
J. Li, C. H. Wen, S. Gauza, R. Lu, S. T. Wu. Refractive indices of liquid crystals for display applications. J. Disp. Technol. 1, 51-61, 2005
Data
Additional information
About Liquid crystals
Liquid crystal (LC) is a state of matter that have properties between those of a conventional liquid and those of a solid crystal.