RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Surlyn A-1601
Smith and Loewenstein 1975: n,k 28.6–200 µm

Wavelength: µm
 (28.5714–200.0000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Ionomer resin manufactured by DuPont under the name Surlyn A-1601.

References

D. R. Smith and E. V. Loewenstein. Optical constants of far infrared materials. 3: plastics. Appl. Opt. 14, 1335-1341 (1975)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Surlyn

Surlyn is the brand name of an ionomer resin created by DuPont, a copolymer of ethylene and methacrylic acid used as a coating and packaging material.

Links