Optical constants of SrTiO3 (Strontium titanate, STO)
Wöhlecke et al. 1977: Amorphous; n 0.3–1.0 µm

Wavelength: µm
 (0.3–1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.7791λ^2}{λ^2-0.16755^2}$$

Conditions

temperature: 300

Notes

Amorphous 1–4 µm thin film. Prepared by RF sputter deposition at 300 K substrate temperature.

References

M. Wöhlecke, V. Marrello, A. Onton. Refractive index of BaTiO3 and SrTiO3 films. J. Appl. Phys. 48, 1748–1750 (1977)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Strontium titanate

Strontium titanate (SrTiO3) is a crystalline solid that is often transparent or pale yellow. It possesses perovskite structure and has garnered significant attention in the field of materials science and solid-state physics due to its intriguing dielectric, ferroelectric, and optical properties. SrTiO3 is widely used as a substrate material for growing high-temperature superconductors, magnetic films, and other oxide thin films. Its high refractive index has also made it popular as a diamond simulant in jewelry, although this use has decreased in favor of more modern materials. In addition, it's used in electronics as a high-k dielectric in DRAM capacitors. The compound can be naturally found in a mineral called perovskite, but most commercial SrTiO3 is synthetically produced.

Other names and variations

  • SrTiO3

Links