Optical constants of SiO (Silicon monoxide)
Fernandez-Perea et al. 2009: n,k 0.00155–0.177 µm
Complex refractive index (n+ik)
Derived optical constants
Notes
Density: 2.17 g/cm3. Film deposited at room temperature.
References
M. Fernández-Perea, M. Vidal-Dasilva, J. I. Larruquert, J. A. Aznárez, J. A. Méndez, E. Gullikson, A. Aquila, R. Soufli. Optical constants of evaporation-deposited silicon monoxide films in the 7.1-800 eV photon energy range. J. Appl. Phys. 105, 113505 (2009) (Numerical data kindly provided by Juan Larruquert)
Data
Additional information
About Silicon monoxide
Silicon monoxide (SiO) is an inorganic compound that is a dark brown or black powder at room temperature. Unlike its stable counterpart silicon dioxide (SiO2), SiO is a highly reactive compound. SiO sublimates (converts directly from a solid to a gas) at elevated temperatures and can further oxidize to SiO2 upon exposure to air. Due to its reactivity, it is typically prepared and handled under controlled conditions. In the realm of thin-film deposition, SiO is utilized for its dielectric properties and as a component for various optical coatings. It's often evaporated in a vacuum to produce films that are used as protective or antireflection coatings in optics and electronics. The ability of SiO to act as a barrier against oxygen and moisture has also garnered interest for potential applications in encapsulating sensitive devices.
Other names and variations
- SiO
- Silicon oxide
Links