Optical constants of SiC (Silicon carbide)
Fischer et al. 2017: 4H-SiC; n(e) 17–150 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=6.346+\frac{3.026λ^2}{λ^2-175.2}$$Conditions
temperature: 293 optical_component: e
Notes
4H-SiC (hexagonal crystal structure); Extraordinary optical constants (e); Room temperature.
References
M. P. Fischer, J. Bühler, G. Fitzky, T. Kurihara, S. Eggert, A. Leitenstorfer, D. Brida. Coherent field transients below 15 THz from phase-matched difference frequency generation in 4H-SiC. Opt. Lett. 42, 2687-2690 (2017)
Data
Additional information
About Silicon carbide
Silicon carbide (SiC) is a robust and hard compound characterized by its high thermal conductivity, high electric field breakdown strength, and high power frequency. Its hardness is second only to diamond, which makes it an ideal material for abrasive applications. SiC possesses excellent thermal stability, allowing it to maintain its structural integrity in high-temperature environments. As a result, it is commonly used in power electronics, especially in high voltage devices, due to its ability to operate at high temperatures. In the realm of optoelectronics, SiC serves as a substrate for LED production, given its beneficial bandgap properties. Furthermore, its thermal and chemical resistance has made it a favored material in automotive applications, specifically for brake discs. In recent years, its transparent nature in some infrared spectra has led to research into its use for transparent armor and windows. Its unique combination of electrical, thermal, and mechanical properties position SiC as a pivotal material for various high-performance applications.
Other names and variations
- SiC
- α-SiC
- 3C-SiC
- β-SiC
Links