Optical constants of Si (Silicon)
Vuye et al. 1993: n,k 0.26–0.83 µm; 20 °C
Complex refractive index (n+ik)
Derived optical constants
Notes
20 °C; Crysal orientation: <111>
References
G. Vuye, S. Fisson, V. Nguyen Van, Y. Wang, J. Rivory, F. Abelès. Temperature dependence of the dielectric function of silicon using in situ spectroscopic ellipsometry. Thin Solid Films 233, 166-170 (1993)
Data
Additional information
About Silicon
Silicon (Si) is a crystalline, brittle element with a bluish-grey metallic luster. It stands as the second most abundant element in the Earth's crust, primarily in the form of silicates and oxides. In its pure form, silicon is employed extensively in the electronics industry for the fabrication of semiconductors, which form the basis of most modern electronic devices. The ability of silicon to act as a substrate for microelectronic devices stems from its semiconductor properties and the potential to precisely dope it with other elements to modify its electrical characteristics. Furthermore, silicon finds use in the photovoltaic industry in solar cells. When it comes to optics, silicon is transparent to infrared light, making it valuable for infrared lenses and other optical components. However, it's opaque to visible light. The material's versatility and abundance have made it integral to many industries, from construction to electronics and beyond
Other names and variations
- Si
- Polycrystalline silicon
- Poly
- Semicrystalline silicon
Links