RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Si (Silicon)
Schinke et al. 2015: n,k 0.25–1.45 µm

Wavelength: µm
 (0.25–1.45)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 295

Notes

Relative uncertainties of the absorption coefficient: 0.4% at 0.250 µm, 11% at 0.6 µm, 1.4% at 1 µm, 12% at 1.2 µm and 180% at 1.45 µm. Temperature: 295 K.

References

  1. C. Schinke, P. C. Peest, J. Schmidt, R. Brendel, K. Bothe, M. R. Vogt, I. Kröger, S. Winter, A. Schirmacher, S. Lim, H. T. Nguyen, D. MacDonald. Uncertainty analysis for the coefficient of band-to-band absorption of crystalline silicon. AIP Advances 5, 67168 (2015)
  2. M. R. Vogt. Development of physical models for the simulation of optical properties of solar cell modules. PhD. Thesis (2015)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Silicon

Silicon (Si) is a crystalline, brittle element with a bluish-grey metallic luster. It stands as the second most abundant element in the Earth's crust, primarily in the form of silicates and oxides. In its pure form, silicon is employed extensively in the electronics industry for the fabrication of semiconductors, which form the basis of most modern electronic devices. The ability of silicon to act as a substrate for microelectronic devices stems from its semiconductor properties and the potential to precisely dope it with other elements to modify its electrical characteristics. Furthermore, silicon finds use in the photovoltaic industry in solar cells. When it comes to optics, silicon is transparent to infrared light, making it valuable for infrared lenses and other optical components. However, it's opaque to visible light. The material's versatility and abundance have made it integral to many industries, from construction to electronics and beyond