Optical constants of Si (Silicon)
Franta et al. 2017: n,k 0.0310–310 µm; 10 K
Complex refractive index (n+ik)
Derived optical constants
Conditions
temperature: 10
Notes
Float zone c-Si; Heterogenous data processing combining ellipsometric and spectrophotometric measurements with refractive index determined in B. J. Frey, D. B. Leviton, T. J. Madison. Temperature-dependent refractive index of silicon and germanium, <a href=\https://doi.org/10.1117/12.672850">*Proc. SPIE 6273, 62732J (2006). Numerical procedures updated in D. Franta, P. Franta, J. Vohánka, M. Čermák, I. Ohlídal. Determination of thicknesses and temperatures of crystalline silicon wafers from optical measurements in the far infrared region, [J. Appl. Phys.* 123, 185707 (2018)](https://doi.org/10.1063/1.5026195). Temperature 10 K."
References
D. Franta, A. Dubroka, C. Wang, A. Giglia, J. Vohánka, P. Franta, I. Ohlídal. Temperature-dependent dispersion model of float zone crystalline silicon, Appl. Surf. Sci. 421, 405-419 (2017) (Numerical data kindly provided by Daniel Franta)
Data
Additional information
About Silicon
Silicon (Si) is a crystalline, brittle element with a bluish-grey metallic luster. It stands as the second most abundant element in the Earth's crust, primarily in the form of silicates and oxides. In its pure form, silicon is employed extensively in the electronics industry for the fabrication of semiconductors, which form the basis of most modern electronic devices. The ability of silicon to act as a substrate for microelectronic devices stems from its semiconductor properties and the potential to precisely dope it with other elements to modify its electrical characteristics. Furthermore, silicon finds use in the photovoltaic industry in solar cells. When it comes to optics, silicon is transparent to infrared light, making it valuable for infrared lenses and other optical components. However, it's opaque to visible light. The material's versatility and abundance have made it integral to many industries, from construction to electronics and beyond
Other names and variations
- Si
- Polycrystalline silicon
- Poly
- Semicrystalline silicon
Links