RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Si (Silicon)
Franta et al. 2013: n,k 0.138–26.9 µm

Wavelength: µm
 (0.138038–26.9153)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Film a-Si:H; Multi-sample method; Heterogenous data processing combining ellipsometric and spectrophotometric measurements on films deposited on c-Si and glass; Experimental data of the films deposited on c=Si are taken from D. Franta, D. Nečas, L. Zajíčková, I. Ohlídal, J, Stuchlík, D. Chvostová. Application of sum rule to the dispersion model of hydrogenated amorphous silicon, <a href=\https://doi.org/10.1016/j.tsf.2013.04.012">*Thin Solid Films* 539, 233-244 (2013). Room temperature."

References

D. Franta, D. Nečas, L. Zajíčková, I. Ohlídal, J, Stuchlík. Advanced modeling for optical characterization of amorphous hydrogenated silicon films, Thin Solid Films 541, 12-16 (2013) (Numerical data kindly provided by Daniel Franta)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Silicon

Silicon (Si) is a crystalline, brittle element with a bluish-grey metallic luster. It stands as the second most abundant element in the Earth's crust, primarily in the form of silicates and oxides. In its pure form, silicon is employed extensively in the electronics industry for the fabrication of semiconductors, which form the basis of most modern electronic devices. The ability of silicon to act as a substrate for microelectronic devices stems from its semiconductor properties and the potential to precisely dope it with other elements to modify its electrical characteristics. Furthermore, silicon finds use in the photovoltaic industry in solar cells. When it comes to optics, silicon is transparent to infrared light, making it valuable for infrared lenses and other optical components. However, it's opaque to visible light. The material's versatility and abundance have made it integral to many industries, from construction to electronics and beyond