Optical constants of Samia ricini (eri silkworm) silk
Perotto et al. 2017: Fibroin film; n 0.3–1.695 µm
Wavelength:
µm
(0.3–1.695)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.475+0.0057λ^{-2}+5\text{×}10^{-5}λ^{-4}$$Notes
Samia ricini (eri silkworm) fibroin film
References
G. Perotto, Y. Zhang, D. Naskar, N. Patel, D. L. Kaplan, S. C. Kundu, F. G. Omenetto. The optical properties of regenerated silk fibroin films obtained from different sources. Appl. Phys. Lett. 111, 103702 (2017)