Optical constants of SCHOTT - Optical glass
FK3

Wavelength: µm
 (0.3–2.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.973346627λ^2}{λ^2-0.00640795469}+\frac{0.146642231λ^2}{λ^2-0.020565293}+\frac{0.679304225λ^2}{λ^2-80.4965389}$$

Conditions

temperature: 293

Notes

inquiry glass

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of FK3

thermal_dispersion:
  - 
    type: formula A
    coefficients: -4.9e-06 1.23e-08 -1.19e-10 3.45e-07 7.72e-10 0.18
nd: 1.4645
Vd: 65.77
glass_code: 464658.227
glass_status: special
density:
  - 
    value: 2270
thermal_expansion:
  - 
    temperature_range: 243 343
    value: 8.2E-6
  - 
    temperature_range: 293 573
    value: 9.4E-6
dPgF: -0.0003
resistance:
  climatic: "2.0"
  stain: "3.0"
  acid: 52.4
  alkali: "2.0"
  phosphate: "1.0"

About SCHOTT AG

SCHOTT AG is a German multinational company renowned for its expertise in specialty glass and glass-ceramics. Founded in 1884, the company has been a pioneer in the field, with innovations that have significantly impacted a variety of industries, including healthcare, home appliances, electronics, and optics. In the optical domain, SCHOTT offers a comprehensive range of high-quality glass types, including crown and flint glasses, as well as specialty materials like laser glasses and radiation-shielding glasses. These materials are used in a myriad of applications, from consumer electronics and camera lenses to scientific instruments and aerospace technologies. SCHOTT's glass products are highly regarded for their quality, consistency, and durability, meeting rigorous industry standards. With a strong focus on research and development, the company has continued to introduce innovative products that address the evolving needs of the optical industry. SCHOTT's commitment to quality and innovation has established it as a leading provider of specialty glass solutions, making it a go-to choice for designers and manufacturers seeking high-performance materials. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.