Optical constants of SCHOTT - Miscellaneous glass
BOROFLOAT® 33

Wavelength: µm
 (0.24–2.800)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=0.3542+\frac{0.78657λ^2}{λ^2-0.10856^2}+\frac{0.18285λ^2}{λ^2-4.427^2}$$

Notes

Room temperature.

References

  1. BOROFLOAT® 33 – Optical Properties, June 2021 (obtained from http://www.schott.com).
    Refractive index: Fit of numerical data with Sellmeier equation - Mikhail Polyanskiy
    Extinction coefficient: Transmission data extracted from figures and converted to k values - Mikhail Polyanskiy
  2. BOROFLOAT® 33 – Technical data, March 2019 (obtained from http://www.schott.com).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of BOROFLOAT® 33

nd: 1.471
Vd: 65.41
density:
  - 
    value: 2230
youngs_modulus:
  - 
    value: 64000000000
poissons_ratio:
  - 
    value: "0.20"
thermal_expansion:
  - 
    temperature_range: 293 573
    value: 3.25E-6
thermal_conductivity:
  - 
    temperature: 363
    value: 1.2
transformation_temperature:
  - 
    value: 798
resistance:
  hydrolytic: 1
  acid: 1
  alkali: 2
hardness:
  - 
    type: Knoop
    value: 4710000000

About SCHOTT AG

SCHOTT AG is a German multinational company renowned for its expertise in specialty glass and glass-ceramics. Founded in 1884, the company has been a pioneer in the field, with innovations that have significantly impacted a variety of industries, including healthcare, home appliances, electronics, and optics. In the optical domain, SCHOTT offers a comprehensive range of high-quality glass types, including crown and flint glasses, as well as specialty materials like laser glasses and radiation-shielding glasses. These materials are used in a myriad of applications, from consumer electronics and camera lenses to scientific instruments and aerospace technologies. SCHOTT's glass products are highly regarded for their quality, consistency, and durability, meeting rigorous industry standards. With a strong focus on research and development, the company has continued to introduce innovative products that address the evolving needs of the optical industry. SCHOTT's commitment to quality and innovation has established it as a leading provider of specialty glass solutions, making it a go-to choice for designers and manufacturers seeking high-performance materials. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.