Optical constants of SCHOTT - Infrared glass (IRG)
IRG 22
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=2.4834+\frac{2.8203λ^2}{λ^2-0.1352}+\frac{0.9773λ^2}{λ^2-1420.7}$$Conditions
temperature: 293
References
Data
Additional information
Properties of IRG 22
thermal_dispersion:
-
type: formula A
coefficients: 6.41e-05 0 0 1.68e-07 0 9.96e-01
density:
-
value: 4410
thermal_expansion:
-
temperature_range: 293 373
value: 1.25E-5
specific_heat:
-
value: 330
thermal_conductivity:
-
value: 0.24
transformation_temperature:
-
value: 641
hardness:
-
type: Knoop
value: 1410000000
fracture_toughness:
-
value: 550000
shear_modulus:
-
value: 8900000000
youngs_modulus:
-
value: 21500000000
About SCHOTT AG
SCHOTT AG is a German multinational company renowned for its expertise in specialty glass and glass-ceramics. Founded in 1884, the company has been a pioneer in the field, with innovations that have significantly impacted a variety of industries, including healthcare, home appliances, electronics, and optics. In the optical domain, SCHOTT offers a comprehensive range of high-quality glass types, including crown and flint glasses, as well as specialty materials like laser glasses and radiation-shielding glasses. These materials are used in a myriad of applications, from consumer electronics and camera lenses to scientific instruments and aerospace technologies. SCHOTT's glass products are highly regarded for their quality, consistency, and durability, meeting rigorous industry standards. With a strong focus on research and development, the company has continued to introduce innovative products that address the evolving needs of the optical industry. SCHOTT's commitment to quality and innovation has established it as a leading provider of specialty glass solutions, making it a go-to choice for designers and manufacturers seeking high-performance materials. SCHOTT also publishes a glass catalog (SCHOTT Optical Glass Datasheets), which is a standard reference for the properties of many optical glasses.