RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of PtAl2 (Platinum-aluminium intermetallic)
Chen and Lynch 1988: n,k 0.22–0.79 µm

Wavelength: µm
 (0.22–0.79)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Bulk sample. Room temperature.

References

L.-Y. Chen and D. W. Lynch. The optical properties of AuAl2 and PtAl2. Phys. Status Solidi B 148, 387-394 (1988) (Data points extracted from a figure)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Intermetallic

Other names and variations

  • Intermetallic compound
  • Intermetallic alloy
  • Ordered intermetallic alloy
  • Long-range-ordered alloy

Links