RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Pr (Praseodymium)
Fernandez-Perea et al. 2008: n,k 0.000775–0.323 µm

Wavelength: µm
 (0.000774901–0.323113894)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Density: 6.773 g/cm3. Film deposited at room temperature.

References

M. Fernández-Perea, M. Vidal-Dasilva, J. A. Aznárez, J. I. Larruquert, J. A. Méndez, L. Poletto, D. Garoli, A. M. Malvezzi, A. Giglia, S. Nannarone. Transmittance and optical constants of Pr films in the 4-1600 eV spectral range. J. Appl. Phys. 103, 113515 (2008) (Numerical data kindly provided by Juan Larruquert)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Praseodymium

Praseodymium (Pr) is a soft, silvery, malleable, and ductile metal that belongs to the lanthanide series of the periodic table. While not as abundant as some other rare earth elements, praseodymium is still found in significant quantities in certain minerals, such as monazite and bastnäsite. In terms of its optical properties, praseodymium is often utilized in the creation of certain types of yellow and green glasses and ceramics, which can absorb ultraviolet light. Additionally, praseodymium-doped fibers have been explored in the realm of fiber optics for their potential use in amplifiers. The metal can also be found in alloys, where it is used to produce high-strength metals that are used in aircraft engines.

Other names and variations

  • Pr

Links