RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Pilkington-Optiwhite (NSG)
Treharne et al. 2011: n,k 0.3–1.5 µm

Wavelength: µm
 (0.30141754–1.4979382)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Variable-angle ellipsometer was used to take amplitude and phase change measurements. The refractive index and extinction coefficient was extracted for NSG Opti-White (low-Fe) glass from a multi-oscillator model fit to the ellipsometry data, as a function of wavelength, from 300 to 1500 nm

References

R. E. Treharne. RF magnetron sputtering of transparent conducting oxides and CdTe/CdS solar cells. PhD Thesis, University of Durham (2011) (Numerical data kindly provided by Dr. Robert Treharne)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information